Add to Cart
Whole epoxy resin worktop with No joints , has large operate space
1. Description
The difference between phenolic resin and epoxy resin is construction materials and manufacturing process. Phenolic resin countertops are composite panels made by layering natural kraft papers that have been saturated with phenolic resin and processed under high heat to form a solid surface composite panel. Epoxy resin countertops are a mixture of resin, silica, a hardener, and filler, which are molded and oven cured as a solid slab.
Functionally, phenolic and epoxy resin countertops are very similar. The main difference is heat handling capacity. As previously mentioned phenolic resin countertops perform very well with continuous heat exposure up to 350°F (176°C). Epoxy resin will handle higher heat loads including open flame.
Molded epoxy resin worktop with marine edge:
No joints for whole worktop, has large operate space and nice appearance.
There is groove on the edge, any of liquids can flow into groove, and very easy for clean groove.
Radius edge is conform to ergonomics, it's comfortable for staff.
Edge: efficetively reduce the potential risk of glassware fall into the ground.
2. Application:
Epoxy resin worktops are use in all kinds of laboratories. In view of the rigid request for laboratory, epoxy resin worktops are vey popular in laboratory industry, it is the best choice for lab staff. The laboratory include the following:
3. Physical Property:
Physical Test Results | |||
No. | Test Item | Test Method | Result |
1 | Compressive Test | ASTM D695-10 | 24000psi |
2 | Deflection Temperature Under Load | ASTM D648-07 Method B | 262℃ |
3 | Density | ASTM D792-13 Method B | 133.8lb/ft3 |
4 | Flexural Strength | ASTM D790-10 Method A | 12200psi |
Flexural Modulus | 2350000psi | ||
5 | Horizontal Burning | ASTM D635-10 | Classification:HB |
6 | Rockwell Hardness | ASTM D785-08 Procudure A | HRM106 |
7 | Water Absorption | ASTM D750-98(2010)e1 | 0.00259% |
8 | High Temperature Resistance Test | _ | No bubbles,rupture,deformation on the surface |
9 | Fire Resistatnce Test | _ | No bubbles,rupture,crack on the surface |
4. Case show: